What is the composition of Linotype?
Table of Contents
The Linotype alloy consists of 4% tin, 12% antimony and 84% lead; each bar measures approximately 8-3/4″ x 1″ x 2″ and weighs approximately 5 lbs (+/- . 25).
What alloy is Linotype?
Linotype or eutectic alloy is a broad name applied to five categories of lead alloys used in manufacture of type, each with three to five sub-classifications. One alloy is composed of lead with 4% tin and 12% antimony.

What is the composition of wheel weights?
Today, the three most common types of wheel weights in use are made from lead, steel or zinc, and are offered in adhesive or clip-on forms. When deciding which one to use, state regulations, environmental factors, material cost and product fitment are a few factors that play a role.
What lead alloy is used in bullets?
Linotype metal
Linotype metal is a eutectic alloy of 3% tin, 12% antimony, and 85% lead. It is a very satisfactory alloy for casting most bullets.
What is the hardness of Linotype?
Linotype is typically known to be too hard for hunting as it will shatter upon bone contact. It is great for high velocity target bullets. Blended 1 to 1 with pure lead, this alloy can produce Hardball alloy. The Brinell Hardness of Linotype alloy is approximately 22.

What is the Brinell Hardness of Linotype?
Very few applications call for an alloy harder than about 15 on the Brinell hardness scale. Many commercial cast bullets run 21-24; Linotype has a nominal hardness of 22.
What are scrap wheel weights worth?
ScrapMonster has become North America’s largest scrap trading platform with 96,513 members and the trusted source for scrap prices, news, and information. Join Today!…Lead Wheel Weights Price.
Region | Price |
---|---|
North America, US East Coast | $0.31 per Lb |
US Midwest, US West Coast | $0.31 per Lb |
Are all wheel weights made of lead?
Most new cars and light trucks sold in the US feature zinc or steel wheel weights, and all new cars and light trucks sold in the US have been free of lead wheel weights since 2009.
What temp does Linotype melt?
Melting Point-Solidus: 237 C, 459 F.
What is the best lead for bullet casting?
Hardball Bullet Casting Alloy consists of 2% tin, 6% antimony and 92% lead. This modern version of the old Lyman #2 is an excellent all-around alloy for most handgun bullets and many higher velocity rifle cartridges.
What is #2 alloy?
Hardball Bullet Casting Alloy consists of 2% tin, 6% antimony and 92% lead. This modern version of the old Lyman #2 is an excellent all-around alloy for most handgun bullets and many higher velocity…
What is antimony lead?
Definition of antimonial lead : lead containing antimony specifically : a hard alloy of lead containing 4 to 10 percent antimony used for the framework of storage-battery plates and tank linings — compare grid metal, hard lead.